Medium Open Extrusion & Hotend

Blob of death and filament leaking around the hotend

When a part detaches mid-print, plastic can build up around the Neptune 4 Pro hotend and encase the heater block and wiring. The thermistor leads are very thin and can snap when the blob is pulled off, after which the printer shows a below-zero temperature and will not heat. Elegoo has a wiki page on this for the Neptune 4 and 4 Pro, and Printer Hub reports Elegoo does not treat it as a warranty case.

What fixes it

Check the cold temperature reading first. Heat to about 200 °C, power off, and pull the blob off while warm without pulling on wires; replace the thermistor if it reads below zero. Re-torque the nozzle hot, then re-level and reset the Z offset. Prevent it with a correct Z offset, a clean plate and supports on small-footprint models.

Log in to confirm this happens to you 0 owners confirmed

Workarounds (0)

No workarounds posted yet.