PLA heat creep clogs with door and lid closed
With PLA on the textured plate (55 °C bed) and the enclosure shut, the chamber can get warm enough for filament to soften above the hotend and jam, especially in a warm room. Bambu's wiki names enclosure heat as the most common clog cause on the P1S and X1 Carbon.
What fixes it
Bambu recommends removing or opening the front door and top cover for PLA, PVA and TPU. Owners also leave the door cracked and a gap at the top glass on long prints.